Saturday, April 25, 2009

[MW:2033] EN 287-1 welder qualification

Hello,

i have the following situation.......

i have to test some welder coming from other sites acc. with EN 287-1........

the question is .....my project is tank erection and facilities .....

if the welder will pass 4" pipe butt weld 6G( h-l045) they will cover
also plates and fillet welds..

thanks

Daniel

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...