Dear Parviz,

You can use similar WPS / procedure for welding A333 grade 6. But in
my opinion it is only possible to use a PQR made in material A106
grade B for welding A333 grade 6 when impact tests are performed on
the test weld. This normally is required for A333 Grade 6 material and
such test is mostly not performed on an A106 grade B test weld.
If there are no impact requirements than you may use the A106 PQR.

Best Regards,

Herman Pieper

On 22 apr, 14:14, parviz farhadi <parvizfarh...@gmail.com> wrote:
> Dear All,
>
> Is it possible to use WPS of ASTM A106 Grade B and its PQR for ASTM A333 Gr
> 6?
>
> Regards,
> Parviz

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...