> No idea about pipes. But the standard method for cleaning copper wire
> rod during wire drawing process is pickling in hot 20% sulfuric acid
> followed by rinsing in water.
>
> Any suggestions from members?
>
> ________________________________
>
> From: venu moturu [mailto:moturuvenu@yahoo.com]
> Sent: Sunday, April 19, 2009 5:30 AM
> To: Bathula Raghuram (Mumbai - PIPING); sanjay
> Subject: cleaning of copper pipes
>
>
>
> Dear Raghu,
>
>
>
> Could you pl. advice/ suggest me any procedure / cleaning method
> available for removing tarnish on copper pipes ....
>
>
>
>
>
> Regards
>
> venu
>
>
>
>
> >
>
DON BOSCO MARITIME ACADEMY
Premier Automobiles Road,
Kurla West, Mumbai 400070
Tel: (022) 2504 1585 / 2018; 25036344. Fax: (022) 2504 0682
Email: donboscomarine@vsnl.net
Website: www.dbma.in
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments