group number is supplementary essential variable ( applicable only when impact test is required )

On 4/10/09, BHARAT GOLE <bharatgole@hotmail.com> wrote:
For SMAW process as per ASME section IX PQR qualified with Base Metal A106 Gr. B to A106 Gr. B i.e P No. 1 Group1 to P No.1 Group 1

Impact  & PWHT not applicable.

Please let me know what is Base Metal Qualified range for WPS...is it P 1 Group 1&2 to P 1 Group1&2   OR  P 1 Group 1 to P 1 Group 1

Regards

Bharat B. Gole




The new Windows Live Messenger. You don't want to miss this. --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...