[MW:1886] RE: 1885] Re: Fillet welding of shell to bottom joint of API 650 Tanks

No such restriction in API. However it states the welding of the shell to the bottom shall be practically completed before the welding of bottom joints that may have been left open to compensate for shrinkage of any welds previously made is completed.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of hamza ahmed
Sent: Tuesday, April 07, 2009 1:25 PM
To: materials-welding@googlegroups.com
Subject: [MW:1885] Re: Fillet welding of shell to bottom joint of API 650 Tanks

 

Hi Mr. Shah,

 

Yes, I totally agree with you. But here due to some fabrication and erection mistake, there is a gap of 10 mm. As per AWS D1.1, upto 5mm can be accepted. As applicabe code is API 650, I wanted to know if there is any reference in this code.

 

With Regards

Ahmed Husain,

ABS TPI

Borouge2

--- On Mon, 4/6/09, shah B.K <b.k.shah@espasia.in> wrote:


From: shah B.K <b.k.shah@espasia.in>
Subject: [MW:1883] Re: Fillet welding of shell to bottom joint of API 650 Tanks
To: materials-welding@googlegroups.com
Date: Monday, April 6, 2009, 11:18 AM

Hello Dear

For shell to bottom weld gap is not required. Shell Plate should be completely contact with bottom plate.

Regards

B.K.Shah

On Sat, Apr 4, 2009 at 1:53 PM, hamza ahmed <ahmraha@yahoo.com> wrote:

Hi,

Can anybody describe the maximum gap allowed between shell to bottom joint of API 650 tank. It is a ' T ' joint requiring fillet weld. Bottom plate thickness is 10 mm and shell plate thickness is 12 mm. Also please descirbe the relevant API 650 or ASME IX paragraph.

 

With Regards.

 

Ahmed



 



 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...