[MW:1078] Re: 1047] thumb rule

Have you tried Ar CO2 mixed gases? What is the gas being used and what is the flow rate
 
regards,
jd






Subject: [MW:1050] RE: 1047] thumb rule
Date: Fri, 22 Aug 2008 10:59:59 +0530
From: R.Bathula@ticb.com
To: materials-welding@googlegroups.com


If ur using Globular you can switch to spray transfer method to reduce spatter,

 

V=20+0.4i   is a thumb rule for SMAW, no idea about GMA.

 

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of mech
Sent: Thursday, August 21, 2008 7:49 PM
To: Materials & Welding
Subject: [MW:1047] thumb rule

 

 

hai friends

 is there any thumb rule to find current and voltage in metal active

gas welding ... v r using semi automatic MAG machine.with   2.4 mm

filler wire dia .current in the rang of 570-670 amps and  voltage

30-39  .and tell wat would b the best way to reduce spattesrs and blow

holes and cracks in this welding .

 

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...