As in the past we found few questions on furnaces and felt to add this to those messages.
Just today I read an interesting second page article in newspaper on Finex furnace which are new generation furnaces without ovens able to operate using fine coal instead of the traditional coking coal which is a high pollutant. Using this furnace the energy cost and pollution is reduced. And yet it does produce the pig iron suitable for high grade steels.
Posco with Siemens, then VAI has developed this in the past 10 years spending heavily and Posco's new plant in India and Vietnam are planned to be build with these Finex furnaces. This is a modification of Corex furnaces as per the article.
They claim the cost is reduced by 10% in overall and as the current fine coal price and coking coal price gap is increasing, they hope it should be more profitable in the coming years.
Good for Nature and Environment and in having a competitive steel price.
Regards,
Kannan. --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment