Monday, August 25, 2008

[MW:1057] RE: 1056] PWHT Furnace

Fuel-Fired Furnaces

 

Advantages:

· Lower energy cost

· Easy to adjust or alter connected input

· Faster heat-up times because inexpensive control factors can be added to accommodate the difference in fuel burned during heat-up

Disadvantages:

· Requires extensive ventilation systems

· Potential explosion or fire hazard

· Requires more manpower for start-up and shutdown

· Adjustment more difficult to maintain, resulting in excessive fuel use

· Only certain materials or types of products can be run in direct-fired furnaces due to the effect of high dew point and oxidizing flue gases on the part surface

 

Electrically Heated Furnaces

 

Advantages:

· Systems are clean and free of the pollution normally found with fuel-fired systems

· Quieter because of the absence of blowers and combustion noise

· More uniform heat pattern

· No exhaust system required; no make-up air system required

· Does not generally require purge or flame safety systems

· Electrical power available almost everywhere

Disadvantages:

· High initial equipment costs

· Higher operating costs

· Cool-down times are longer because no combustion air is available

 

Source: ASM

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Chetan Parekh
Sent: Monday, August 25, 2008 2:00 AM
To: materials-welding@googlegroups.com
Subject: [MW:1056] PWHT Furnace

 

Hi Friends,

 

I need comparision between gas fired furncae and electrical induction heating furnace. Basically I am looking for advantage and disadvantage between these two heating media.

 

Regards,

 

Chetan Parekh

Abu Dhabi



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS