Dear Dave
 
Babu n carlos are right, u can weld any fillet, in any diameter as per QW451.1 if you have qualification as per /qw451.1 n qw 451.2.
 
You can weld in short
 
Shabbir

On Wed, Aug 20, 2008 at 6:39 PM, babu raghavan <babuprmech@yahoo.com> wrote:
Mr: S.N.DAVE CHECK ASME SECTION IX  QW 451.4.You can see the details.This welder can weld 3/4 " socket weld.
 
BABU.P.R
 


--- On Fri, 8/15/08, shailesh dave <snd2988@yahoo.com> wrote:
From: shailesh dave <snd2988@yahoo.com>
Subject: [MW:1034] Re: LIMIT OF WELDER QUALIFICATION OVER DIA. RANGE Date: Friday, August 15, 2008, 8:47 AM


Dear Romio,
 
It is ASME SEC. IX.
 
Regards,
 
S.N.Dave

--- On Thu, 8/14/08, romio dabre <romiomdabre@gmail.com> wrote:
From: romio dabre <romiomdabre@gmail.com>
Subject: [MW:1032] Re: LIMIT OF WELDER QUALIFICATION OVER DIA. RANGE
To: materials-welding@googlegroups.com
Date: Thursday, August 14, 2008, 5:10 PM

please write the code? As per ASME sec IX it is not allowed

On Wed, Aug 13, 2008 at 12:11 PM, shailesh dave <snd2988@yahoo.com> wrote:
DEAR MEMBERS,
 
I HAVE COME ACROSS AN INTERESTING SITUATION.
 
WE HAVE WELDERS QUALIFIED IN 6" x 7.11 mm THK. PIPE OFF COURSE BUTT WELD. MY QUESTION IS CAN THESE WELDER PERFORM WELDING OF SMALL BORE PIPE LIKE 3/4" SOCKET WELD.
 
PL. HELP ME.
 
REGARDS,
 
S.N.DAVE
 
QA/QC INCHARGE
ADGAS, DAS ISLAND, UAE










--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...