Dear Carlos,
I presume you are referring the Table 331.1.1 in ASME B 31.3. This table cross refers the PWHT requirement for different P group materials. The specified hardness limits (in the last column of the table) are only applicable for the welds & HAZ as per 331.1.7 (a).
The intent of the code is, Wherever the hardness values are not specified (Px groups), the hardness testing need not to be carry out after Heat treatment for those materials.
 
If your query is about the acceptable hardness limits for a particular P1 group material, then you have to look the relevant material specification.(for e.g. A 234 WPB, - 197 HB, A 105 187 HB etc)
 
I hope this will clarify the query.
 
Regards,
Sanjeevan
----- Original Message -----
Sent: Saturday, August 16, 2008 8:31 AM
Subject: [MW:1037] Re: [MW:1036]

less than 220 BHN
Tagore

 
On 8/15/08, carlosoliveros@terra.com <carlosoliveros@terra.com> wrote:
DEARS FRIENDS, I AM WANTED ABOUT HARDNESS TEST FROM P1, ASME B31.3 WRITTE THE VALUES P3,P4,P5 AND OTHERS BUT P1 IS NOT COMMENTED
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...