Friday, August 15, 2008

[MW:1035] Re: LIMIT OF WELDER QUALIFICATION OVER DIA. RANGE


Yes, the welders can to weld all fillet welds because , if  your qualification was buttweld(groove-joint)

carlosoliveros@terra.com




On Thu 14/08/08 07:40 , "romio dabre" romiomdabre@gmail.com sent:

please write the code? As per ASME sec IX it is not allowed

On Wed, Aug 13, 2008 at 12:11 PM, shailesh dave <snd2988@yahoo.com> wrote:
DEAR MEMBERS,
 
I HAVE COME ACROSS AN INTERESTING SITUATION.
 
WE HAVE WELDERS QUALIFIED IN 6" x 7.11 mm THK. PIPE OFF COURSE BUTT WELD. MY QUESTION IS CAN THESE WELDER PERFORM WELDING OF SMALL BORE PIPE LIKE 3/4" SOCKET WELD.
 
PL. HELP ME.
 
REGARDS,
 
S.N.DAVE
 
QA/QC INCHARGE
ADGAS, DAS ISLAND, UAE







--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...