Thursday, August 14, 2008

[MW:1031] Re: Impact Test as per EN875 & EN10045-1-Reg

YES . ASME Sec VIII Div.1 allows reduction in energy values for sub size s[pecimen.
Refer to the code.
Tagore

 
On 8/13/08, Kumaran <kums@godrej.com> wrote:
Dear all,
 
When v r doing impact test using sub size specimens on weld as per above stds,
Is there any value  reduction of absorbed energy specified? or v need to meet the values required for the full size(10x10mm) impact specimens?
 
If anyone had any such previuos experiences ..plz suggest..
 
Regards
B.Kumaran
Welding Department,
Godrej & Boyce Mfg. Co. Ltd,
Mumbai,
INDIA
Ph: +912267964527
Fax: +912267961514

and service. We will be glad to be of assistance to you.

* Toll free number available in Ahmedabad, Bangalore, Chennai, Delhi, Hyderabad,
Kolkata, Lucknow, Mumbai, and Pune

" Visit our website - http://www.godrej.com "
=======================================================================




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...