Dear all,
 
When v r doing impact test using sub size specimens on weld as per above stds,
Is there any value  reduction of absorbed energy specified? or v need to meet the values required for the full size(10x10mm) impact specimens?
 
If anyone had any such previuos experiences ..plz suggest..
 
Regards
B.Kumaran
Welding Department,
Godrej & Boyce Mfg. Co. Ltd,
Mumbai,
INDIA
Ph: +912267964527
Fax: +912267961514

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...