[MW:1014] RE: 1013] PURPOSE OF TAKING RADIOGRAPHY OF SOCKET WELD JOINT.

To check the gap (see figure 328.5.2C of ASME B31.3)

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of shailesh dave
Sent: Monday, August 11, 2008 8:54 AM
To: materials-welding@googlegroups.com
Subject: [MW:1013] PURPOSE OF TAKING RADIOGRAPHY OF SOCKET WELD JOINT.

 

DEAR MEMBERS,

 

CAN ANYBODY LET ME KNOW FOR WHAT PURPOSE WE ARE CONDUCTING THE RADIOGRAPHY OF SOCKET WELD JOINTS.

 

REGARDS,

 

SAILESH

 

I/C QA/QC

 

ADGAS, DAS ISLAND UAE




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...