Within the contest of valves, I have used the valve seating nitrided to achieve very high hardness in special cracking furnace gate valves.(Not the usual gates)
The surface nitriding does have effect on the phy. property change as well.

With regards,
Kannan



Sudipto_Banerjee@fwuk.fwc.com
Sent by: materials-welding@googlegroups.com

08/08/2008 10:34

Please respond to
materials-welding@googlegroups.com

To
materials-welding@googlegroups.com
cc
Subject
[MW:1008] Material query for SS 304N






Hi friends,
Pls. let me know may be in what circumstances SS 304N is used in place of
SS 304 or 304L.


Best Regards,
Sudipto Banerjee
Equipment Engg. Department
Office no. 0044- (0)118 913 2295


=======================================================
Confidentiality Notice

This communication and the information it contains:-
(a) Is intended for the person(s) or organisation(s) named above and for no other person(s) or organisation(s).  
(b) May be confidential, legally privileged and protected in law. Unauthorised use, copying or disclosure of any of it may be unlawful. If you have received this communication in error, please contact us immediately by email at Postmaster@fwuk.fwc.com.
=======================================================



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...