Thursday, August 7, 2008

[MW:1001] RE: 998] Re: Equivalent Material

If you can do RT on the welds, you can even try for on the job qualification for performance


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of SENTHILKUMAR SWAMINATHAN
Sent: Thursday, August 07, 2008 2:05 PM
To: materials-welding@googlegroups.com
Subject: [MW:998] Re: Equivalent Material

 

Thanks Sanjeevan,

Welder qualification as per ASME IX.

API 5L X56 is equal to All combination of P1 - P11, P34, P4X and unassigned metal of similar chemical composition to these metals. Please clarify.

 

Regrads,

S.Senthilkumar

--- On Thu, 7/8/08, Quality <quality@gpsoman.com> wrote:

From: Quality <quality@gpsoman.com>
Subject: [MW:997] Re: Equivalent Material
To: materials-welding@googlegroups.com
Date: Thursday, 7 August, 2008, 11:18 AM

Senthil,

Welder qualification as per which code ASME sec IX or API 1104 or any other standard/specification?

Normally Grade/ strength of material is not an essential variable for welder performance qualification.

Nearly equivalent material is A 381 Grade Y56 (S1 Group) & A 671 grade CK75 (p1 group).

 

best regards,

Sanjeevan

----- Original Message -----

Sent: Thursday, August 07, 2008 9:25 AM

Subject: [MW:996] Equivalent Material

 

Dear Sir,


1) I want to conduct Welder qualification test on this pipe material API 5L X56, what is equivalent material in ASME? Due to non availability of Actual material

2) I want to conduct Welder qualification test on this plate material BS EN 10025 Part 3 S355 NL material, what is equivalent material in ASME? Due to non availability of Actual material

skumarswami@yahoo.co.in 

 

Regards,

S.Senthilkumar

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs