Monday, April 15, 2013

Re: [MW:17410] WPS

Yes you can use Impact tested WPS/PQR for non-impact test requiring jobs.
 
Thanks & Regards

J.Gerald Jayakumar
00968-99438165
From: Ahmed Husain <ahmraha@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Sunday, April 14, 2013 9:43 PM
Subject: [MW:17393] WPS

Dear All,
 
Your valuable comment is required on following cases.
 
1. Suppose, if i have a certified PQR for P1 Gr1 to P1Gr1 material with PWHT and impact testing. Process is GTAW and SMAW. Based on this PQR, can I prepare a WPS without impact testing, i.e for materials and design condition doesn't require impact testing. There is no issue in other variables.
2. Is it acceptable to apply a 'WPS prepared and approved for low temperature service with impact testing ' to a job, for which there is no requirement for impact testing.
 
A. Husain
ABS Consulting Inc.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...