[MW:5355] ER316 & E316-16 FOR CRYOGENIC SERVICE

Dear all,
 
 
one of our Client specification says"Qualification on Material Gr.316 also qualifies for Gr.316L but not Vice versa"
 
I want to esatblish WPS for Stainless steel Material Gr.316 (cryogrnic service) as per B31.3
 
 
My query is
 
whether  ER316 for GTAW Process and E316-16 for SMAW  will meet the Impact requirement?
 
 
Regards,
S.Veloumany
 
 
 
 
 

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...