Dear Sir, 

It is a condensate receiver tank and it is a design requirement from client side.

Regards, 
Saravanan. 
S.KOREA 

On Thu, 22 May 2025, 9:26 pm Raghuram Bathula, <raghurambathula@gmail.com> wrote:
Why do you use P22 nozzles on CS?

On Thu, 22 May 2025, 16:24 PARAI Reaction Channel, <saravanshyla@gmail.com> wrote:

Dear Sirs ,

 

We have a project with both shell and Reinforcement Pad materials SA516-70, 10 mm Thk ( P No.1 ) and the Nozzle is SA335-P22, 4" Sch 120 , 

11.1 mm ( P No.5A ) Thk.

 We already have a qualified WPS & PQR with 8mm GTAW and tested about 10 years ago by other welding engineer, for P No,.5A to P No.1 without PWHT and it was satisfactorily passed and we 

have used that WPS & PQR for the previous project 10 years ago and no 

issues found without PWHT.

 Now for the new project, we are going to use the same WPS and apply 

Preheat ( 204 to 250 Deg C ) as per the WPS for 10mm Shell Thk by 

multipass welding, refer to the below sketches.





So, i would like to confirm whether PWHT is mandatory as per UCS-56-4 ?

Can we avoid PWHT for this 10mm weld joint ?


Or Should we do buttering with ERNiCr-3 on P No.5A bevel and butt weld 

with same filler for this dissimilar joint to avoid PWHT after making new 

PQR with buttering?


Please confirm soon.


Thanks and Regards,

Saravanan Sornam,

ANSAN-Si,

S.Korea 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CALV1rk%2Biby3LDhuASFD6Sx3wD6mhOVKRXA8dsJCQcfO-yNsjhQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CADxVub%3DgSEPtoFpp%2BtcafrEOrNOzUxFt_9E4TfiPwfyP21JHdg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CALV1rkJt_cnVR3wJkwRy%3DHUD9Qviu-HO7EmcYVbQQmmkV2v8iA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...