Re: [MW:35619] PWHT

Dear Elavarsan 

As per B31.3

A preheat of 95°C (200°F) is applied prior to welding on any nominal material thickness >25 mm (>1.0 in.)
Multiple layer welds are used when the nominal material thickness >5 mm (>3 16 in.) [Single-layer or single-pass welds may be exempted from PWHT, provided the WPS has been qualified using single - pass welds with ±10%heat input and that all other conditions for exemption are met.]

Depends on Your WPS

On Fri, May 16, 2025 at 10:35 AM Elavarasan Mech <elavarasan1861994@gmail.com> wrote:
Dear all

please clarify below 

As per B31.3 above 16 mm ( P1 MATERIAL)thickness required PWHT?
what's is minimum thickness required for PWHT as per B31.3 ( P1 MATERIAL)

Regard 
ELAVARASAN 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4yk4GW_Uq%2BhMu7hnqcq5NCEgu5%3D1ckMpLjLKZu2THbDKJQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAGAT7zdo4QFC2R09qe_3xNWd1VE23u_i0cUumoXJE9DfWKW_%3Dg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...