This is small Pipe welding.
Pl use GTAW process full welding .
SMAW is not to be used .
Sent from my iPhone

On 12 May 2025, at 12:17 PM, ananth karuppanan <ananthkaruppanan91@gmail.com> wrote:


Dear,

ERNiCrMo -3 backing temperature max 350 Deg.C. Can you try min backing temp 320 Deg. C and 2 hours must. For the welding consumables brand better go with Special Metals. 

Thanks & Regards,
Ananth Karuppanan.
Mobile : +91-9597936444
               +971-588925593


On Mon, 12 May 2025 at 1:26 PM, patni engineers <patniengineers@gmail.com> wrote:
BACKING  FILLER WIRE ?

On Mon, May 12, 2025 at 2:42 PM Subrata Das <subrata19732111@gmail.com> wrote:
Dear Expart,

Can you please guide on the steps to follow to weld UNS 31254 Pipe to Forging. We are facing much issue on weld finish and slag inclusion. We are using ERNiCrMo3 & ERNiCrMo3 consumables with 200 Deg.C backing and 70-80 Amp current. Please refer the attached photo of the welded joint. 

Thanks in advance,
Subrata Das
9828160168

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/212db25d-02eb-4254-9bc5-5141f368fa2fn%40googlegroups.com.


--
Regards,

Chandrakant
B.E Mech.
ASNT Level II RT/UT/PT/MPT/CSWIP

GST -27AMOPP5962A1ZS
Patni Engineers. Mumbai. India
PED/2014/68/EU
welding shop AD2000/DIN EN ISO 3834
IBR Approved 

Factory Addreess- Pl Call 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAKLNAG7TBbkstRpnMhX7JcNDGUN8dR%3DMr__AJ7zU%3DtwruboE%3DA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAMK7HtDX_XjDu7iVx-L%2Bm8T2p0teBWMv7O4UxExtNmWesz2Vvg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...