Re: [MW:35591] Clarification on WPS Applicability for SS316L to Duplex Welding per ASME Section IX

Thanks Vishwas sir, let me check with Customer specification once again. 

Best Regards, 
Nambirajan A

On Fri, 2 May, 2025, 5:30 am Vishwas Keskar, <vvkeskar123@gmail.com> wrote:
P10 H to P8 
ASME sec IX 
WPS is acceptable
If API582 or other Client specifications are applicable , then revisit the decision.
Review Discuss with QA ,Welding proceed accordingly 
Sent from my iPhone

On 1 May 2025, at 11:32 PM, Deerendra Karanth <dkaranths@gmail.com> wrote:



If supplementary requirements for impact testing are applicable, a change in A-number will require new WPS qualification; however, if impact testing is not required, the existing WPS can be used as long as the P-Number and F-Number remain unchanged.

BR, 

Deerendra.. 



On Thu, 1 May, 2025, 18:57 Nambirajan Avudaiappan, <nambirajanavudaiappan@gmail.com> wrote:
Dear ranijith,
My question regarding the applicability of WPS only.

On Thu, 1 May 2025 at 14:03, Ranjit singh <ranjit450@gmail.com> wrote:
Dear sir,

We are facing problem in welding crack for desimilar metal like en19 hub dia 350mm thick 200mm and shaft en19 dia 140mm groove weld 28mm.

Process:- SMAW
Pre heating 200-250 degree.
Observation:- crack 

Regards,

Ranjit
9216671043

On Thu, May 1, 2025, 1:40 PM Nambirajan Avudaiappan <nambirajanavudaiappan@gmail.com> wrote:

Dear Experts,

I hope this message finds you well.

I would like to seek your clarification regarding the applicability of an existing WPS.

We have successfully qualified a WPS for welding SS316L to Super Duplex using ER2594 filler metal. Both base materials are classified under P-No. 8 to 10H, and the filler metal falls under F-No. 6.

However, our actual production requirement involves welding SS316L to Duplex Stainless Steel using ER2209, which also falls under F-No. 6, and the base metals remain under P-No. 8 to 10H.

As per ASME Section IX, since the base metal P-Numbers and filler metal F-Numbers remain unchanged, could you please confirm whether the existing WPS is valid for this application as well, or if a new qualification is required?

Thank you in advance for your guidance and support.

Regards,

Nambirajan A

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJuyB2XnCz1x1PWFoGvwdFQQCG-e_8K_ksgtNPtt2mwocbS4Gw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CA%2BE2JLO6r4aNeUGLsCJdcKXpwF9ju6wthJoEpub5-PSiZ6fovQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJuyB2UjQfSLHGNbtSCDYfzsxxoD_sQ84Jqih_CO5xa1Xxu3Sg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAG0nF9Fv%2B8%3DAGFvJ05Ajkccw42bVAQDc9J72x63gy9XHnGmBcg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/B892992F-4859-4742-BEEA-A914C99D39E8%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJuyB2X4fM9FduqALkH4jBYH6ZL06J7pu7vfZ-y2ysLMqMaxhQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...