Re: [MW:35587] Clarification on WPS Applicability for SS316L to Duplex Welding per ASME Section IX

Dear sir,

We are facing problem in welding crack for desimilar metal like en19 hub dia 350mm thick 200mm and shaft en19 dia 140mm groove weld 28mm.

Process:- SMAW
Pre heating 200-250 degree.
Observation:- crack 

Regards,

Ranjit
9216671043

On Thu, May 1, 2025, 1:40 PM Nambirajan Avudaiappan <nambirajanavudaiappan@gmail.com> wrote:

Dear Experts,

I hope this message finds you well.

I would like to seek your clarification regarding the applicability of an existing WPS.

We have successfully qualified a WPS for welding SS316L to Super Duplex using ER2594 filler metal. Both base materials are classified under P-No. 8 to 10H, and the filler metal falls under F-No. 6.

However, our actual production requirement involves welding SS316L to Duplex Stainless Steel using ER2209, which also falls under F-No. 6, and the base metals remain under P-No. 8 to 10H.

As per ASME Section IX, since the base metal P-Numbers and filler metal F-Numbers remain unchanged, could you please confirm whether the existing WPS is valid for this application as well, or if a new qualification is required?

Thank you in advance for your guidance and support.

Regards,

Nambirajan A

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJuyB2XnCz1x1PWFoGvwdFQQCG-e_8K_ksgtNPtt2mwocbS4Gw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CA%2BE2JLO6r4aNeUGLsCJdcKXpwF9ju6wthJoEpub5-PSiZ6fovQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...