Friday, May 2, 2025

Re: [MW:35573] SS FILLER

agree

On Wed, 23 Apr 2025 at 18:32, venkateswara reddy Desireddy <dvreddy82@gmail.com> wrote:
If essential variables doesn't change , and impact not applicable, then you can use WPS.



On Wed, 23 Apr 2025, 4:58 pm Elavarasan Mech, <elavarasan1861994@gmail.com> wrote:
Dear All 
 Please clarify below 

we have qualified WPS( P No 8 GR 1 To P NO 8 GR 1). Filler metal Er 316l ( Fno:6)
 
In our current project UNS S31254 ( PNO 8 Gr No 4)
We useing a filler wire ER2594 (Fno 6 )


Can we use above wps for this project with filler metal ER2594  Please guide me 
CODE ASME SEC IX 





regards 
ELAVARASAN

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ymviaYs8wTi0ZC2v_L9PsxT9%3DRsHdQNgCDbJJSZsjdyug%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEabyK%3DS3fUCDDqn-Mq0nFx_a5T4%2BFcUJvig6jQcc-FTyN1urA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29Oh9X75ccZnSesRGJPD6qY%2BKRvY8dGzvbNacXxgPcumX-A%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...