Re: [MW:35559] SS FILLER

It is a typo error as was mentioned correctly in the last line.

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Thursday 24 April, 2025 at 09:03:19 am IST, Vishwas Keskar <vvkeskar123@gmail.com> wrote:



The plate designation seems to be wrong
UNS 312254
The designation shall be 
SA 240 UNS 31254
Pl correct if I am wrong .
Pl mention what is service process application ?
For TYP31254 , ERNiCRMo10 shall be used if PREN  required is higher and pitting corrosion is prime requirement 
Vishwas
9823472273
IWE

Sent from my iPhone

On 23 Apr 2025, at 9:23 PM, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:


UNS 312254 falls under the category of Super Austenitic stainless steel and commonly know as 6Mo alloy or 254SMO.

The Filler wire you are using ER 2594 is not correct and it  is for Super Duplex stainless steel with alloying ellements on lower side.

The correct Filler metal to weld UNS 31254 is  ERNicrMo3 for which the F-No is 43 and hence you cannot use the existing WPS.

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Wednesday 23 April, 2025 at 04:58:05 pm IST, Elavarasan Mech <elavarasan1861994@gmail.com> wrote:


Dear All 
 Please clarify below 

we have qualified WPS( P No 8 GR 1 To P NO 8 GR 1). Filler metal Er 316l ( Fno:6)
 
In our current project UNS S31254 ( PNO 8 Gr No 4)
We useing a filler wire ER2594 (Fno 6 )


Can we use above wps for this project with filler metal ER2594  Please guide me 
CODE ASME SEC IX 





regards 
ELAVARASAN

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ymviaYs8wTi0ZC2v_L9PsxT9%3DRsHdQNgCDbJJSZsjdyug%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1743224755.492666.1745422825229%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit
https://groups.google.com/d/msgid/materials-welding/028FA6F3-304E-4804-804B-554CEF9C0735%40gmail.com
.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...