Dear Experts,

I hope this message finds you well.

I would like to seek your clarification regarding the applicability of an existing WPS.

We have successfully qualified a WPS for welding SS316L to Super Duplex using ER2594 filler metal. Both base materials are classified under P-No. 8 to 10H, and the filler metal falls under F-No. 6.

However, our actual production requirement involves welding SS316L to Duplex Stainless Steel using ER2209, which also falls under F-No. 6, and the base metals remain under P-No. 8 to 10H.

As per ASME Section IX, since the base metal P-Numbers and filler metal F-Numbers remain unchanged, could you please confirm whether the existing WPS is valid for this application as well, or if a new qualification is required?

Thank you in advance for your guidance and support.

Regards,

Nambirajan A

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJuyB2XnCz1x1PWFoGvwdFQQCG-e_8K_ksgtNPtt2mwocbS4Gw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...