[MW:35544] WELDING OF SS 310 MATERIAL CRACK ISUUE..

We are doing a welding of SS 310 Material Plate with ER310 Grade welding electrode... But its contineous cracking.... at welding line,,,,...? Kindly Guide if any one..

IS ANY ALTERNATE WELDING MATERIAL CAN BE USED...?
IS ANY SPECIAL PROCEDURE TO WELD THIS MATERIAL...?

PRAVIN