Skip to main content

RE: [MW:32069] Welder Qualification API 1104

Hi TKD Yokesh,

 

I believe this requirement included in API 1104, 2020 edition, clause 6.1, which is still in the draft stage, not yet approved and published. This means this Code is yet to be a legal document. I did not see this clause being mentioned in 2018 or earlier versions.

Anyway, the answer to your query is as below. This sounds sensible , when each welder is welding half- circumference of the pipe. That's not the case when 2 welders weld on the same coupon, each of them welding the entire circumference.

 

Thanks.

 

 

 

Pradip Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Vaishakh Kc
Sent: March 17, 2021 10:55 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:32066] Welder Qualification API 1104

 

Which code permits to do wpq like this?

 

On Wed, 17 Mar 2021, 13:52 TDK YOKESH, <tdky167@gmail.com> wrote:

Dear experts,

 

I am qualifying 2 welder on 20" pipeline. One half welder by welder A and other half welder B.  The RT result shows Welder A side failed and Welder B side passed.

Query : Both the welders are rejected as the coupon has failed or should I consider welder A and welder B passed.

 

Any code reference or interpretation on similar case will be helpful. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKT-TuovOFQLQmMRN17eosER4WP1cMtcEWQb%2BRhiAnvmaEG7EA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGnSN%3DJdgHuaNL9SRea-Sx_8rL%3DViKO0JFc522b_y5fbbRuxDw%40mail.gmail.com.


Virus-free. www.avg.com

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .