[MW:32023] RE: FCAW substitute for SMAW in offshore platforms

Hi

FCAW is one of the approved welding processes for offshore construction. Often restrictions are imposed by the end user/client. You need to go by what your project/client specification calls for. Here're some industry specific documents for your reference. GMAW is also a reliable process, however type of the process, i.e.  short circuit/ globular/spray arc decides the application and the effectiveness of this technique.

By and large of the processes are far more accomplished than what they were ,15-20 years ago.

 

Hope these attachments will provide the general insights on your query.

 

Regards.

 

 

 

Pradip Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Saudi Aramco Approved Designated Welding Engineer(DPWR)

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

From: EmaD FaRaHanI <emad.farahani@gmail.com>
Sent: March 5, 2021 12:01 PM
To: materials-welding@googlegroups.com
Subject: FCAW substitute for SMAW in offshore platforms

 

Dear All,

I want to replace SMAW in the fabrication of offshore platforms, top side section.

In this regard, FCAW is selected mainly for most of the welds, to increase the speed of fabrication.

May I know:

1- Is FCAW the right choice? how about GMAW?

2- In the case of FCAW, which electrode with a 3.2mm size is proper for all position welding in offshore platforms? mainly high strength steels

 

Regards,

E.F


Virus-free. www.avg.com

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .