Re: [MW:31377] Unlisted Material AWS D1.1

U can contact material for welding procedure. They give some inputs which will be useful. Generally root Welding is done under match filler metal and other layer matched filler material. Preheat is based on thickness and CE. Over preheat will reduce the Hardness. This is not coming under preview of D1.1, u can follow it's procedure. 

On Tue, 1 Sep 2020 1:45 am , <pgoswami@rogers.com> wrote:

Hardox, is an abrasion resistant steel, not very commonly used for structural fabrication. Here're two data sheets which tells almost the same story .

 

Welding   considerations for this steels are quite tricky and requires very high level of preheat .  To the best of my knowledge structural codes does not incorporate use of such abrasion resistant  steel. If this material is acceptable for construction you should ask the WPS to supported by a qualified PQR form welding approval  prior to production.

 

Thanks.

 

 

Pradip Goswami, P.Eng, IWE

Consultant-Welding-Metallurgical Engineering

 

Cell & Whatsapp-905-9793232.

Personal:pgoswami@rogers.com

 

 

 

 

 

From: Kannayeram Gnanapandithan <kgpandithan@gmail.com>
Sent: August 31, 2020 11:53 AM
To: materials-welding <materials-welding@googlegroups.com>
Subject: Re: [MW:31373] Unlisted Material AWS D1.1

 

Only hardness other strength not guaranteed

 

On Mon, 31 Aug 2020 8:14 pm Vishwas Keskar, <vvkeskar123@gmail.com> wrote:

Request them to furnish Mechanical properties

They will furnish 

No issue at all 

 

On Mon, 31 Aug 2020, 18:27 jaimin...@gmail.com, <jaiminthejack@gmail.com> wrote:

Dear Gents,

 

I got one WPS for  hardox 450 

 

Required Code: AWS D1.1

Plate Thk: 25mm

 

My concern is that as per given Data sheet there is not specified Tensile Strength ,on what basis we can accept Report of Tensile Test?

 

This is my first experience with unlisted material.

 

Thanks & Regards

Jaimin Patel
B.E Mechanical

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/46b74d37-8ccf-40dd-ab4e-dda0b27073e7n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3OM-KTP9YMPK2gWcMKsEBAj8uOwvhjw4HuHRpowW4Jn%3Dg%40mail.gmail.com.


Virus-free. www.avg.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAAAhissbuC7PQrXdaBlEBjUVAQAAAAA%3D%40rogers.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNVWE6_2mXd9bR8EfJGcAPbjztaV-2Re6yTSrk-6fQp1Q%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...