Re: [MW:31243] Welder qualified in API1104 Standard with destructive testing re destructive test require for station piping.(sec-ix)

Required DT & RT. 
Regards, 
S.SENTHILKUMAR 


On Fri, 31 Jul 2020 at 2:32, HARISH VARUDE
<harish.varude02@gmail.com> wrote:
Respected all experts,

I have one welder who qualified in API standard (for line pipe,gas field)with DT reports but now we want to do his new qualification for station piping as per Section ix Standard,for his qualification destructive test again require or not.
Or radiography base we can qualify to him.

From
Herish varude
Mob.No.:-7990746918

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGP-YKLrY6EtcSGS%2Bqi_fBfMDSemr7awiFkDuACDb4EUoCSNfQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1780025937.7867180.1596164493187%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...