You can qualify your welder with guided bend tests or radiography, although there are some P numbers that require only guided bend.
Regards!.

El jue., 30 jul. 2020 a las 20:26, HARISH VARUDE (<harish.varude02@gmail.com>) escribió:
Respected all experts,

I have one welder who qualified in API standard (for line pipe,gas field)with DT reports but now we want to do his new qualification for station piping as per Section ix Standard,for his qualification destructive test again require or not.
Or radiography base we can qualify to him.

From
Herish varude
Mob.No.:-7990746918

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGP-YKLrY6EtcSGS%2Bqi_fBfMDSemr7awiFkDuACDb4EUoCSNfQ%40mail.gmail.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SUMMIT MÉXICO - TPI

https://www.linkedin.com/in/summit-m%C3%A9xico-tpi-760047137/

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5Zur%2BHL1%2B54s%3DSUvAqFwjd6NP23V%2BLda5ek9KKiR7hUXbn-Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...