Hi Chris,

You are right. The positions in brazing hase been defined based on flow. Please refer QB-460 (you might have already referred.

Thanks,
Best Regards,
Rajnish Dixit
On Monday, 27 July, 2020, 04:40:09 pm GMT+7, chris <chrissabu28@gmail.com> wrote:


Hi all;

Can i qualify a fillet joint by brazing. I can't find the suitable clause in ASME QB section.
Please advise.

Regards

Chris

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/027f91a7-b19c-4b96-bce7-6b11c18e8abfo%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1978166472.6585199.1596106519828%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...