Thursday, July 30, 2020

Re: [MW:31237] Eccentric Reducer (Fitting to fitting) Seam Orentation


Please discuss with client to get the actual situation approval.




என்றும் அன்புடன்,
Thanks & Regards,
RAJAVARMAN
+971561895584

On Tue, Jul 21, 2020, 4:54 PM 'Dinesh' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear all,

Eccentric Reducer (Fitting to fitting)  fit up, seam matching as below,

In this case,what is requirement need to follow and what is exact reason to do 1 inch. flushing on seam .

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/baf9d41c-0489-493e-8699-7acebc37e5bdn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BHpzU6bKD5D7HrmkTRrCd%2BOoLsvLSL-%2BMEEjhSSJepiA04mtw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...