Re: [MW:31227] Welder qualification for CS and SS

For welder qualification, SS backing gas  is invariably classed as an essential variable. This is because being able to produce a sound weld root using backing does not demonstrate he has skill required to make a sound weld without backing.

On Tuesday, 28 July 2020, 07:41:55 EEST, José Juan Jiménez Alejandro <jjjimeneza@gmail.com> wrote:


The answer of 

Kannayeram Gnanapandithan

is correct.

El lun., 27 jul. 2020 a las 10:10, 'anand gupta' via Materials & Welding (<materials-welding@googlegroups.com>) escribió:
Dear
Please check F No is same then welder can weld cs and ss.

Regards
A p gupta
Thyssekrupp


On Sun, 26 Jul 2020 at 7:50 PM, Venkat Ramana
Hi Experts,

My query is once welder was qualified for CS material, can he weld for SS also.... 

Please advise

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHAXWsN5Yzfq036c3S4fumVeSKUo8HgZxbpkSu-daMchAShF5w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1638992183.6508832.1595847435919%40mail.yahoo.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5Zur%2BBR87OknkoX-6xy3wguenfhMAxkf2950teq2wE5JgmSw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...