Hi,

Yes, Piping requirements.

SA 516 gr 60/70. and according to ASME Sec.IX and ASME B31.3.
The main PQR is qualified with PWHT, but not HIC tested.
And I have additional PQR with HIC tested, but not qualified with PWHT, and no other lab test reports like a mechanical test, bend test, and hardness test report, shall I combined this PQR to my WPS.

Please looking you feedback.
Thanks 
Kiran



On Tuesday, July 28, 2020 at 10:12:01 AM UTC+5:30, Sudhakar Kuppuswamy wrote:
Hi,

Please specify the material grade and the design code. 

As you have mentioned Line class, I presume you are talking about piping . 

Regards 
Sudhakar K 

On Mon, 27 Jul 2020 at 11:33 AM, K K <kara...@gmail.com> wrote:

Hi Experts,


"Good Morning"


According to my line classes, I required NACE+HIC+PWHT Wet H2 services.

What is the test shall be conducted according to the standard to meet the requirements?


I have one PQR with NACE+PWHT+Wet H2S services, but not HIC test.

In addition, I have qualified one HIC tested PQR without PWHT no other lab test certificates, shall I combined this PQR to the above requirements( NACE+HIC+PWHT+wet H2S).

For your information, the HIC test is an additional requirement of our specifications.

Please looking your feedback on my above query.


Thanks and Regards

Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f1d53635-4e0f-4fe5-a0cf-ec93a8d2d87bo%40googlegroups.com.
--

Regards,

Sudhakar K CEng MWeldI,IWE.

Welding & Metallurgical Engineer,

Email: sudhak...@gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/036721c7-5728-4727-b92a-ad48067f8453o%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...