Re: [MW:31220] Welder qualification for CS and SS

yes u r absolutely right no doubt but whats about remaining essential variable sec 9 does mentio only reffer p number essential variable

On Mon, 27 Jul 2020, 7:11 pm Kannayeram Gnanapandithan, <kgpandithan@gmail.com> wrote:
pl ref ASME sec IX- QW 423.1
(Any one Pno between Pno1-Pno15E, qualify from Pno1 to Pno15E)

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Jul 27, 2020 at 2:44 PM Raja Varman <peraiyur.varman@gmail.com> wrote:

When P no. change, need new qualification.


என்றும் அன்புடன்,

Best regards,

RAJAVARMAN SELVARAJ

+971561895584



On Mon, Jul 27, 2020 at 8:10 AM Venkat Ramana <venkatgps.ramana@gmail.com> wrote:
ASME Sec IX

On Sun, Jul 26, 2020, 8:37 PM José Juan Jiménez Alejandro <jjjimeneza@gmail.com> wrote:
It is important that you describe what code you are using, each standard has its advantages and limitations.

El dom., 26 jul. 2020 a las 9:19, Venkat Ramana (<venkatgps.ramana@gmail.com>) escribió:
Hi Experts,

My query is once welder was qualified for CS material, can he weld for SS also.... 

Please advise

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHAXWsN5Yzfq036c3S4fumVeSKUo8HgZxbpkSu-daMchAShF5w%40mail.gmail.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza






Libre de virus. www.avast.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurJ0PzACcC%2BVD%3DJnqHFkzO7s6ykJ0N%3DD8SABNia2xL40Wg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHAXWsOUJcn%2B3WHLfNe8VK_0Nc_S7pX_3aBGjzReLimuJhZGjA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BHpzU4Hf4-Nh%3DDSgu8RUpfeVhJHwfn9FmDe1eTvmjLXc-gYvw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePEd2LbnX_ox3ut0dL%3Dm%3DxjPV4tBTnYrm5ek%2BeTVSqrEQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOWr6k_yCZ4EdSxJpG8NMY1%2By8ruQF_kF25CoLG0z8QOxN57OQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...