Re: [MW:31215] Annealing and Normalizing temperature for F316 & SS410

There is no normailzing for ASS

Στις Τετ, 22 Ιουλ 2020 στις 6:50 π.μ., ο/η SURESH <qms.pjgpl@gmail.com> έγραψε:
Dear Experts
Kindly let us know the Annealing and Normalizing temperature for below material grade

1.ASTM A473 Typ410- Annealing and Normalizing temperature

2.ASTM A182 F316- Solution Annealing and Normalizing temperature


Kindly let us know this temperature is anywhere mentioned in the standard


Regards
Suresh kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/306f0eff-a199-4621-877a-ae4d49bb9b45o%40googlegroups.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CFfA8-wQygdvJ7FDBT94dh5fp_Hk2aJOASOasm7F25jA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...