Monday, July 27, 2020

Re: [MW:31212] SA 312 TP304 for SA 312 TP 304L

how to give purging for 3 meter dia shell to weld of SA316 Gr 240L material with GMAW (tig).

On Thursday, 16 July 2020 12:09:25 UTC+5:30, Dharma dattu wrote:
Thanks you all 

Question 1:  WPS was established in 2008, can it be used now?

Question 2: for a 3 meter dia tank how to give purging to do root weld with GTAW.

On Tuesday, 7 July 2020 12:19:39 UTC+5:30, Rajavarman wrote:
Hi.

Both are same P.no8/Group.no1.

So no issue to use the old WPS.
But must be consider,

1. Special requirements other essential variables such as thickness range, 
And supplimentry essential variables,
Based on particular project requirements.

2. Approval of new client.



என்றும் அன்புடன்,
Thanks & Regards,
RAJAVARMAN
+971561895584

On Tue, Jul 7, 2020, 9:29 AM Dharma dattu <dharm...@gmail.com> wrote:
Hello All,

We have a new project for which main components are SA 312 TP 304L material, currently we have SA 312 TP 304 WPS can we ues the same, as the Pno. is same!

Regards,
Dharma Dattu. B

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/89ae66ad-2aad-40ce-aed3-fe009c801617o%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/54b1da84-770d-4f2f-9553-a3a4cc4974f1o%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...