Monday, July 27, 2020

Re: [MW:31211] Welder qualification for CS and SS

Base metal qualified provided other essential variable are to be verified. 

On Mon, 27 Jul 2020 1:03 pm Venkat Ramana, <venkatgps.ramana@gmail.com> wrote:
Can you please advise with code or general industrial practices.. 

On Mon, Jul 27, 2020, 9:40 AM 'Rajnish Dixit' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Answer is a big NO.


On Sun, 26 Jul 2020 at 21:47, Venkat Ramana
Hi Experts,

My query is once welder was qualified for CS material, can he weld for SS also.... 

Please advise

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHAXWsN5Yzfq036c3S4fumVeSKUo8HgZxbpkSu-daMchAShF5w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1452474133.5146218.1595777319617%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHAXWsMjk-E-6u7LitweUuW_Re7%2BWpwZaY4%3Dp8CgDO%2B_dfJcKQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNU%2B87AXuQ81FnaSHFaKE8Oz5imq7_ER4gmgQh7Z58XXA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...