Dear  Suresh,

does your client require these heat treatments for the raw material or after the fabrication (e.g. after welding)...?
please share more details.

Regards
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Thu, Jul 23, 2020 at 9:32 AM SURESH <qms.pjgpl@gmail.com> wrote:
Thanks Mr.Ramon Briceno

But my client is suggesting to do annealing for ASTM A473 Typ410 at the temperature of 950 C (Customer mentioned TDC). Is there any adverse effect on the change of hardness?

Regards
Suresh Kumar

On Wednesday, 22 July 2020 09:20:32 UTC+5:30, SURESH wrote:
Dear Experts
Kindly let us know the Annealing and Normalizing temperature for below material grade

1.ASTM A473 Typ410- Annealing and Normalizing temperature

2.ASTM A182 F316- Solution Annealing and Normalizing temperature


Kindly let us know this temperature is anywhere mentioned in the standard


Regards
Suresh kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e83a51c2-3ea3-44e7-9c07-180156d3d5d9o%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUj%2Bw%2Bp7uX4V35%2BhQpPAYb-mLxrDTconGS4-HnOQU%3DN_2Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...