Re: [MW:31170] API 6A MONOGRAMMED COMPONENTS MATERIAL CLASS

Matl Chemistry  requirement.is.to be controlled.as.specified


On Tue, 21 Jul 2020 at 19:38, Prakash Hegde
<pb.hegde@yahoo.com> wrote:


Hl
Yes material mech properties e.g if you select ASTM 4130
YS OF 75ksi min
65ksi  is specified in API spec
Hardness restriction is same.for.all grade