Dear Brother,

As per API 1104, Rolled to Fixed or Vice Versa require Requalification.for Procedure.

Hence WPS Does not Qualifies for 2G Position.

But WPS do qualify 6G Position. Hence Welder qualificaton can be done in 6G Position.

Please Find the screenshot of the Same



Hnce 
With Regards,

Sandeep.P.Raghavan


On Mon, Jul 20, 2020 at 9:05 AM HARISH VARUDE <harish.varude02@gmail.com> wrote:
As API 1104 specifications

From
Herish varude
Mob.No.:-7990746918

On Mon, Jul 20, 2020, 10:17 AM HARISH VARUDE <harish.varude02@gmail.com> wrote:
Dear all,

Contractor have a Approved WPS in 5G position and now he want to do weld joints in 2G position and also want to welder qualification in 6G position.
Can it possible???

From
Herish varude
Mob.No.:-7990746918

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGP-YK%2B69MY7CMiRy1yKR2gKcD%2B-W4r%2B1RCNBU%3DNvZ%3D6simwHw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFBEtQqQqt-XtP3qfRRqODUDDi2vD4uiGq3JTi6_ZCA7uu%2Bg7w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGP-YKJo3ChXvoRrjhke2D2YkB%3DV7De2DqbXhpcNVeHZBzQQ_Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...