Dear Experts,

The same things need WPS qualification range codes and standards

regards
M.LOGANATHAN

On Friday, 6 May 2011 01:11:26 UTC+3, Надежда Бомко wrote:



Dear experts,

Please clarify what requirement for qualification WPS  for fillet weld  Weldolet  PNo 1 Gr.2 to pipe  PNo 1 Gr.1 by ASME section IX. I need defined the range extend for thickness of weldolet.

 Thanks & regards .
Nadya.
--

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c8ea0ce1-7dd8-4a00-a529-f4e77d3d6aaco%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...