[MW:31220] Re: Impact test requirements for LAS

Dear Experts,

Please look into my query, please give me your response on my doubt.

Thanks
 Kiran 

On Monday, July 27, 2020 at 11:29:05 AM UTC+5:30, K K wrote:
Hi Experts,

"Good Morning"

My query has below.

Help me to prepare pWPS.
Process : GTAW +SMAW
Material : P.No - 5B   
ASTM A335 Grade P9.
Pipe Size - 16" Sch-60.
Thickness: 16.66 mm
Thickness range: 5mm to 33.32 mm
According to ASME B31.3 Table 323.3.1 shall I required an Impact for the above-mentioned thickness and material.
As per my knowledge, the above 25 mm impact test would be required. 
How I can find according to line class where impact test required or not.
If a minus 29° C impact test not required for LAS.
 
When we shall consider the impact test exemption. 

And regarding consumable for P No- 5A 
ASTM A335 Grade P22

if I use ER90S-B3 ok or shall I use ER80S-B3 because my client suggest me to use ER80S-B3 please clarify way?

Thanks in advance 

Regards
Kiran




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a5e2843d-2285-4e82-b631-6b73ea0b5aceo%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...