Friday, July 24, 2020

[MW:31189] Re: PWHT Technician'sTraining Requirements

In Canada, Alberta, there are a formal Training but it's only one level "Field Heat Treatment Technician", in UK there are another in 3 levels for CSWIP "Requirements for Certification of Site and Workshop Heat Treatment Operatives"... AWS is still working in "D10.23M/D10.23, Specification for the Qualification of Personnel for Local Heat Treatment of Welds in Pipe and Tube Components"

Saludos

El miércoles, 7 de abril de 2010, 3:03:21 (UTC-5), subr...@batelco.com.bh escribió:

Is there any reference specifications/standards or guidelines related to
training and qualifying PWHT technicians.In the absence of above how to
document their training/qualifications.

Subramani.

--------------------------------------------------------------------
mail2web - Check your email from the web at
http://link.mail2web.com/mail2web


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d155df40-8ef7-4e83-99da-c6a2126b0328o%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...