Friday, July 24, 2020

[MW:31185] Re: Annealing and Normalizing temperature for F316 & SS410

Dear Mr.Ramon Briceno,
I am going to use it for machining only. Required hardness is 160BHN

So for ASTM A473 Typ410 can we suggest annealing temperature of 950 C for 1hour/inch soaking and furnace cooling?


Regards
SURESH

On Wednesday, July 22, 2020 at 9:20:32 AM UTC+5:30, SURESH wrote:
Dear Experts
Kindly let us know the Annealing and Normalizing temperature for below material grade

1.ASTM A473 Typ410- Annealing and Normalizing temperature

2.ASTM A182 F316- Solution Annealing and Normalizing temperature


Kindly let us know this temperature is anywhere mentioned in the standard


Regards
Suresh kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/956b41b5-8178-4d94-931c-b5caa4c8f7dao%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...