Monday, July 20, 2020

[MW:31157] WPS qualified in 5G and Welder qualification required in 6G

Dear all,

Contractor have a Approved WPS in 5G position and now he want to do weld joints in 2G position and also want to welder qualification in 6G position.
Can it possible???

From
Herish varude
Mob.No.:-7990746918

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGP-YKJ3%3DWja7crOUryugTZegznOUpe%2BsEZAbs9DBdOY-EOKwQ%40mail.gmail.com.