Tuesday, April 28, 2020

Re: [MW:30824] Tube to Tube sheet welding, Orbital welding parameters for header box

David thank you for your reply. Can you tell me the reasoning behind slower weld speed.

On Thursday, April 9, 2020 at 5:31:09 AM UTC-5, d...@btinternet.com wrote:


Try a slower welding speed and a closer arc length.

Regards, 9 4 2020.