Re: [MW:30749] Can i weld A36 or equivalent S275JR with E7018-B2L?

7018-1 itself will work for-43°C

On Tue, 14 Apr 2020 9:38 am 'james gerald' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
From the Material ASTM A36 and 275JR I understand they are not LTCS material.

try E 7018C2L or E 7018C1L with the maximum carbon of 0.05% and welding consumable MTC will show lower amounts.

Inline image

It also depends on the number of Joints you intend to weld,

Thanks & Regards

J.Gerald Jayakumar




On Monday, April 13, 2020, 07:17:44 PM GMT+7, Chris Sabu <chrissabu28@gmail.com> wrote:


hi james,

They really don't have any impact test requirement which is weird though. They require carbon content less than .04% and elevated nickel content.
I don't see any variation with both these parameters.


On Mon, Apr 13, 2020 at 8:56 AM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
What is your MDMT (minimum Design Metal temperature) at which Impact test to be conducted.

Try E 7018-C3L as it provides Impact test upto to -50degC and also contains Nickel.

E 7018-B2L is a chromium Molybdenum electrode which do not contain much Nickel

Thanks & Regards

J.Gerald Jayakumar



On Monday, April 13, 2020, 10:46:39 AM GMT+7, chris <chrissabu28@gmail.com> wrote:


our customer specifies ultra low carbon content with elevated nickel. Is there any other welding that i can use in this case?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f52cfb16-c52a-436a-a0af-7437a3aa51c8%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/361481876.3065893.1586752043677%40mail.yahoo.com.


--
THANKS AND REGARDS
CHRIS SABU
0559695451

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACY3QXTPfXh6y0uyBh81X-YodFeDpSnG3xTf9T0SY4ALvmxFdQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1247802736.3267726.1586791298688%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePMNfRpB3%3DXhuLYZSeH1tvbPQouyFBaeC4fZ4P%3DjTPD0w%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...